1. Visual Inspection and Macroscopic Morphological Analysis
Surface Defects:
Cracks: Linear or spiral cracks on the inner and outer surfaces, depth ≥1mm, with sharp ends.
Folds: Continuous or discontinuous overlapping in a linear/spiral shape on the outer or inner surface, often caused by original defects in the tube blank or improper grinding.
Hairline cracks: Fine, hair-like cracks on the outer surface, with a spiral direction opposite to the rotation of the piercing mill, related to poor steel quality or incomplete cleaning.
Tool-assisted inspection: Use a magnifying glass or endoscope to observe hidden areas, such as the blind area at the tube end.
2. Non-destructive Testing Techniques
Ultrasonic Testing (UT):
Longitudinal cracks: Using transverse wave external circumferential testing, the sound beam propagates along the circumference of the pipe wall.
Transverse cracks: Using transverse wave external axial testing, the sound beam propagates axially.
Folds/Laminations: Longitudinal wave dual-crystal straight probe testing, high sensitivity.
Eddy Current Testing (ET): Sensitive to surface point defects, suitable for rapid screening.
Magnetic Particle Testing (MT): Detection of surface cracks in ferromagnetic materials, requires magnetization equipment.
3. Metallographic and Microscopic Analysis
Metallographic examination: After sampling and etching, observe the decarburized layer, banded structure, and inclusions (such as sulfides, aluminum oxide).
Scanning Electron Microscopy (SEM): Analyze the microscopic morphology of cracks, distinguishing between high-temperature cracks (such as decarburized layers) and mechanical stress cracks.
4. Process Performance Verification
Flattening/Flaring Test: Simulates the deformation process, exposing folds or crack defects.
Hardness Testing: Abnormal hardness areas may be accompanied by microscopic cracks.