1. Material Composition and Metallographic Analysis
Carbon Equivalent (CE): Excessive carbon or alloying elements (such as Cr, Mo) can easily lead to brittleness. The content of C, Si, Mn, etc., needs to be detected using a spectrometer.
Metallographic Structure: Observe whether the grains are coarse or if abnormal phases (such as martensite, bainite) are present. Brittle materials often show cleavage fracture characteristics.
2. Low-Temperature Toughness Testing
Impact Test: Measure the Charpy impact energy (Akv) below -20℃. If it is lower than 27J (20 ft·lbf), there is a risk of brittleness.
NDT Temperature: Determine the nil-ductility transition temperature through a drop-weight test to ensure that the design temperature is higher than the NDT value.
3. Mechanical Performance Verification
Tensile Test: The elongation after fracture of brittle materials is usually <5%, and the fracture surface is crystalline.
Hardness Test: Brinell hardness (HB) > 200 may indicate a tendency towards brittleness.
4. Environmental and Process Influences
Hydrogen Embrittlement/Stress Corrosion: In acidic environments or after electroplating, the hydrogen content needs to be tested to avoid delayed fracture.
Processing-Induced Embrittlement: Excessive cold deformation or improper heat treatment (such as insufficient tempering) will reduce toughness.
5. Non-Destructive Testing
Ultrasonic Testing: Internal cracks or delamination will show as high reflection signals and must comply with the GB/T5777 standard.